STS 12mm Construction Boards will lose some strength when et. Multiple texts have been carried out which included a pull through test at control conditions when the boards were dry and a pull through test after the boards were immersed in 23°C water for 7 days. There was a slight loss in strength when the boards were tested after immersion, howeverm when they reverted to their dry state, almost all strength had been retained.